[Author Prev][Author Next][Thread Prev][Thread Next][Author Index][Thread Index]
ATM 12 micron blues
I'm a little confused on the fine grind / smoothing stageand need some advice. I'm using
Aluminum Oxide 12 micron, and can't seem to avoid getting "stuck glops of white stuff" on
the mirror and tool - smooth motion is not possible. Tex's, Berry's, or Ellison's
approaches all seem to lead to this - as well as any combination of their approaches.
The problem is water - how much?
What's my objective- a dry grind (virtually no water) or a thin, wet, white, thick fluid
(premix a paste and grind till it starts to grab?
Thanks!
Chris Fuld