[Author Prev][Author Next][Thread Prev][Thread Next][Author Index][Thread Index]
Re[2]: [ATM] Melting Pitch
Hi Mike,
Tuesday, June 14, 2005, 7:14:22 PM, you wrote:
ML> Gugolz Melting Pt Flash Pt Burn Pt Softening Pt
ML> 55-Very Soft 52°-55°C 246°C 278°C 63°-64°C
ML> 64-Soft 68°-72°C 229°C 262°C 65°-68°C
ML> 73-Medium 77°-80°C 219°C 254°C 71°-74°C
ML> 82-Hard 79°-82°C 210°C 246°C 75°-77°C
ML> 91-Very Hard 84°-87°C 213°C 252°C 78°C
Very useful Mike, thanks.
ML> (Meller Optics, Inc.) indicates that Gugolz is wood resin based,
ML> not coal tar based
Very odd - the manufacturers of Gugolz say it's coal tar based.
--
Best regards,
Richard in the UK
_______________________________________________
ATM mailing list http://www.atmlist.net/