At 80 grit, it takes quite a bit of water to make the glass seem translucent
while at 5 micron the surface will be that way by breathing on it and when dry
it should have the appearance of a fresh "satin finish" paint job.
Ken Hunter
(KB7H)
On Tue, 03 Dec 2002 20:33:26 -0500 wayne hilliard <woodycxd@adelphia.net>
wrote:
>
> Hi all a quick question. I've been grinding my
> 10 inch port hole glass
> and have worked my way up to 12 micron. How
> clear should the glass look
> at the 12 and 5 micron stage? I've been
> checking for pit size with a
> loupe and flashlight but am just wondering how
> the glass should appear...
>
> Thanks a bunch...
>
> Wayne Hilliard "If computers are making
> the world a global village,
> KA1CXD FN32 and I can't figure out
> how to use one, does that
> woodycxd@adelphia.net make me the global
> village idiot ?"
>
> Shoe
>
>
>
>
>